Supreme 42HT-2ND
Two component epoxy system for bonding, sealing and coating
Key Features
- Paste consistency
- Convenient processing
- Superior thermal cycling capabilities
- Outstanding temperature and chemical resistance
- Meets NASA low outgassing specifications
- Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
paste
Cure Schedule
overnight at 75°F followed by 3-5 hours at 160-200°F
Hardness
75-85 Shore D
Service Temperature Range
-80°F to +450°F
Glass Transition Temperature (Tg)
130-135°C
Volume Resistivity
>10¹⁴ ohm-cm