UV10TK
One component, moderate viscosity UV curable system for bonding, sealing and encapsulating
Key Features
- Outstanding optical clarity
- High glass transition temperature
- Can cure up to 1/4 inch thick
- Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
6,000-8,000 cps
Cure Schedule
20-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts per cm²
Hardness
>65 Shore D
Coefficient of Thermal Expansion
55-60 in/in X 10⁻⁶°C
Dielectric Constant
3.5
Glass Transition Temperature (Tg)
75-80°C
Refractive Index
1.557
Volume Resistivity
>10¹⁴ ohm-cm