UV10TK40M
One component, higher viscosity UV curable system for bonding, sealing and coating
Key Features
- Outstanding optical clarity
- High glass transition temperature
- Passes NASA low outgassing specifications
- Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
30,000-60,000 cps
Cure Schedule
cures readily in 20-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with 20-40 milliwatts per cm²
Hardness
75-85 Shore D
Service Temperature Range
-60°F to +450°F
Glass Transition Temperature (Tg)
135-140°C
Refractive Index
1.55