UV22DC80-1

One component, nanosilica filled, dual cure system with UV and heat curing mechanisms
Key Features
  • Low viscosity
  • Minimal shrinkage upon curing
  • Superb optical clarity
  • Cures at 80°C in shadowed out areas
Typical Properties
Viscosity
500-3,500 cps
Cure Schedule
Dual cure UV and heat at 80°C, Cures at 80°C in shadowed out areas, Areas not cured because of shadowing can be cured at 80°C for 40-60 minutes, Post curing at 125-150°C for 15-30 minutes can increase the glass transition temperature (Tg) from 90°C achieved by straight UV curing to over 125°C
Hardness
80-90 Shore D
Service Temperature Range
-100°F to +350°F
Coefficient of Thermal Expansion
30-35 x 10⁻⁶ in/in/°C
Refractive Index
1.52
Immagine
UV22DC80-1 UV Curable System
Certifications

Meets EU Directive 2015/863

ASTM E595 Compliant

Video

Product Spotlight: UV22DC80-1

Master Bond UV22DC80-1 is a one part nanosilica filled system for bonding, sealing and coating applications in the aerospace, optical and electronic industries. This video demonstrates the epoxy based system’s unique dual curing mechanism of b …
Product Description

Master Bond UV22DC80-1 is a nanosilica filled, dual cure epoxy based system. It is formulated to cure readily upon exposure to UV light and most importantly it will crosslink in shadowed out areas with the addition of heat. The logic in developing this kind of product is that UV curables will cross-link rapidly and thoroughly upon exposure to the light, but it will not cure in areas where the material is not exposed to the light. Having a dual cure mechanism allows those areas not exposed to the light being curable with the addition of heat. The thermal part of the cure is achieved at a user friendly 80°C (particularly when working with plastics). Dual cure systems are particularly useful for rapidly fixturing parts with the UV portion of the cure and then finishing the process by heating.

This lower viscosity system features a cationic cure mechanism (for the UV portion). This combined with being a nano filled system confers an exceptionally low shrinkage and outstanding dimensional stability. UV22DC80-1 is not oxygen inhibited. After polymerizing, it has many advantageous properties. It bonds well to a wide variety of substrates including metals, glass, ceramics and most plastics. UV22DC80-1 has very good chemical resistance to many acids, bases, fuels and solvents. It is a superb electrical insulator, also it is able to withstand rigorous thermal cycling. The service temperature range is -100°F to +350°F. Straight UV curing can be accomplished for thicknesses of 0.01-0.02 inches in seconds using UV light at 365 nm with 20-40 milliwatts/cm2 of energy. Faster cures can be achieved at higher energy outputs. Areas not cured because of shadowing can be cured at 80°C for 40-60 minutes. In addition, post curing at 125-150°C for 15-30 minutes can increase the glass transition temperature (Tg) from 90°C achieved by straight UV curing to over 125°C. The combination of an 80°C secondary cure and the presence of a nano filler imparts very special properties to this compound. The ability to initiate curing with a UV light source and complete it with heat opens new horizons for the use of UV22DC80-1 in high tech applications particularly in aerospace, optical and opto-electronics, among others.

Product Advantages

  • One component system; no mixing needed
  • Dual curing mechanism allows for curing in shadowed out areas and rapid fixturing time at 80°C
  • No oxygen inhibition
  • Bonds well to a wide variety of substrates
  • Excellent physical strength properties
  • Nano filled, high dimensional stability
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.