UV25TK

One part, medium viscosity UV curable system featuring high temperature resistance

Key Features
  • Superb physical strength properties
  • Unsurpassed chemical resistance
  • Glass transition temperature exceeding 180°C
  • Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
30,000-70,000 cps
Cure Schedule
UV25TK cures readily in 20-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts per cm².
Hardness
85 Shore D
Service Temperature Range
-60°F to +500°F [-51°C to +260°C]
Glass Transition Temperature (Tg)
180-185°C
Volume Resistivity
>10¹⁴ ohm-cm
Image
Certifications

Meets EU Directive 2015/863

1,000 Hours at 85°C/85% RH

Product Description

Master Bond UV25TK is a one part UV curing system for bonding, sealing, coating and encapsulation with optical clarity and excellent physical properties. Most importantly it has a high glass transition temperature and extraordinary chemical resistance. UV25TK cures readily in 20-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts per cm². The rate of cure depends upon the compound’s distance from the light source, the thickness of the section and the intensity of the light source. It should be noted that the system can cure in sections up to 0.010-0.020 inches. However, when bonding, sections of a few thousandths of an inch are more than adequate. Master Bond UV25TK is not oxygen inhibited and therefore does not require any special treatment in that regard. It bonds well to glass, surface treated metals and plastics such as polycarbonates and acrylics, among others. UV25TK is not only effective for bonding applications, it can also be used as a coating, sealant or encapsulant. Its chemical and temperature resistance are truly amazing. UV25TK’s exceptionally high Tg of 180–185°C (TMA) exceeds that of many conventional UV-curable epoxy systems, providing enhanced thermal stability for demanding applications. As noted below in the chemical resistance chart, it withstands long-term exposure to some super aggressive solvents and related entities. The system does not contain any solvents or volatiles and features low shrinkage upon curing. Its service temperature range is -60°F to +500°F. UV25TK is a specialty type UV with a premium for chemical and temperature resistance, thus, it is a prime candidate for applications in aerospace, electronic, optical, specialty OEM and related industries. Particular attention should be paid to the information in the storage and handling section of this data sheet. 

Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.