Top 5 - Low CTE Adhesives
EP21TCHT-1 EPOXY RESISTS CRYOGENIC/HIGH TEMPERATURES Click to request TDS for EP21TCHT-1 Visit our extensive resource library for the latest videos, white papers and tech tips! Thermal conductivity, 75°F Mixed viscosity, 75°F Volume resistivity, 75°F CTE, 75°F 10 BTU•in/ft 2 •hr•°F Thixotropic paste >10 14 ohm-cm 18-20 x 10 -6 in/in/°C Easy to apply • NASA low outgassing approved • Withstands 1,000 hours 85°C/85% RH CONTACT US +1.201.343.8983