Top 5 - Dual Curing Adhesive Systems
UV15DC80Med ONE COMPONENT, BIOCOMPATIBLE EPOXY SYSTEM Click to request TDS for UV15DC80Med UV22DC80-1Med NANOSILICA FILLED, BIOCOMPATIBLE ADHESIVE • Meets ISO 10993-5 and USP Class VI requirements • High dimensional stability • Superb optical clarity Click to request TDS for UV22DC80-1Med Viscosity, 75°F Refractive index, 75°F Dielectric constant, 75°F, 60 Hz Service temperature range 45,000-60,000 cps 1.52 3.5 -60°F to +400°F • Meets USP Class VI requirements • Passes ISO 10993-5 cytotoxicity testing • Excellent physical strength properties Viscosity, 75°F Hardness, 75°F Glass transition temperature with post cure Service temperature range 500-3,500 cps 80-90 Shore D >125°C -60°F to +350°F