Top 5 - High Temperature Resistant Adhesives
EP17HT-LO ONE PART, STRUCTURAL EPOXY COMPOUND Click to request TDS for EP17HT-LO EP42HT-2 TWO PART, CHEMICALLY RESISTANT EPOXY • Heat, chemical and steam resistant • Cures at ambient or elevated temperatures • Solvent free compoud Click to request TDS for EP42HT-2 Glass transition temperature (Tg) Hardness, 75°F Lap shear strength, aluminum to aluminum, 75°F Service temperature range 225°C >80 Shore D 3,200 psi -80°F to +650°F Extremely high glass transition temperature • Meets NASA low outgassing speci cations • Excellent compressive/tensile strength properties Tensile strength, 75°F Tensile modulus, 75°F Index of refraction Service temperature range >12,000 psi 350,000-400,000 psi 1.63 -60°F to +450°F