Top 5 - High Temperature Resistant Adhesives
EP46HT-1AO TWO PART, THERMALLY CONDUCTIVE EPOXY Click to request TDS for EP46HT-1AO MasterSil 800 ONE COMPONENT, SILICONE ELASTOMER SYSTEM • Non-corrosive cures • One part, moisture curing system • Extremely fast set-up time Click to request TDS for MasterSil 800 Thermal conductivity, 75°F Volume resistivity, 75°F Tensile strength, 75°F Service temperature range 9-10 BTU•in/ft •hr•°F >10 16 ohm-cm 7,000-8,000 psi -100°F to +550°F • Meets NASA low outgassing speci cations • Meets MIL-STD-883J Section 3.5.2 for thermal stability • Withstands 1,000 hours 85°C/85% RH Elongation, 75°F Viscosity, 75°F Tack-free time, 75°F Service temperature range 250-350% 35,000-65,000 cps 15-20 minutes -103°F to +572°F