Top 5 - Epoxies for Underfill Applications
EP62-1LPSPMed TWO PART, MEDICAL GRADE EPOXY SYSTEM Click to request TDS for EP62-1LPSPMed EP114 TWO PART, NANOSILICA FILLED EPOXY COMPOUND • Low viscosity and very long open time • Meets NASA low outgassing speci cations • Exceptionally low shrinkage upon curing Click to request TDS for EP114 Tensile strength, 75°F Hardness after 1,000 hours 85°C/85% RH Service temperature range Volume resistivity, 75°F 11,000-12,000 psi 85 Shore D 4K to +400°F >10 14 ohm-cm • Passes USP Class VI and ISO 10993-5 requirements • Capable of resisting repeated sterilization • Very long open time at room temperature Coefficient of thermal expansion, 75°F Compressive strength, 75°F Service temperature range Abrasion resistance, CS-17 wheel, 1,000 cycles 20-22 x 10 -6 in/in/°C 24,000-26,000 psi -100°F to +550°F 5.3 mg