Top 5 - Epoxies for Underfill Applications
EP29LPTCHT TWO PART, LOW EXOTHERM EPOXY SYSTEM Click to request TDS for EP29LPTCHT Visit our extensive resource library for the latest videos, white papers and tech tips! • Applicable in very thin bond lines • Excellent ow properties • Superior dimensional stability CONTACT US +1.201.343.8983
[email protected] www.masterbond.com Thermal conductivity, 75°F Volume resistivity, 75°F Service temperature range Working life after mixing at 75°F; 100 gram batch 9-10 BTU•in/(ft •hr•°F) >10 15 ohm-cm -60°F to +350°F 10-12 hours