The following is a news release from Master Bond Inc. You have received it because you are listed as an editor for your publication.
Attached to this email is a low resolution version of the photograph that is included in the press kit for this product.
High resolution version of this image and files with the body text of this release in Word, HTML and text formats are available at http://www.masterbond.com/newsrelease/ep39maoht.
-----------------------------------------------------------------

FOR IMMEDIATE RELEASE

Thermally Conductive, Electrically Insulative Epoxy Delivers Low Exotherm for Large Castings and Potting Applications

Master Bond EP39MAOHT is a room temperature curing system for demanding bonding, sealing, coating, potting and encapsulation applications. “It is a versatile product that combines convenient handing, good flow, thermal conductivity, electrical insulation and high temperature resistance,” said Robert Michaels, vice president of technical support. “Its toughness lessens the chance of stress cracking when thermally cycled and its low exotherm makes it particularly useful for mid-to-large sized potting applications.”

EP39MAOHT has a low mixed viscosity of 3,000-6,000 cps as well as a convenient one to one mix ratio by weight and a long working life of 120-150 minutes for a 100 gram batch. This dimensionally stable system bonds well to a wide variety of substrates including metals, ceramics, composites and glass as well as many rubbers and plastics with very low shrinkage upon curing.

This formulation features reliable thermal conductivity of 9-10 BTU•in/ft2•hr•°F [1.30-1.44 W/(m•K)], while retaining superior electrical insulation properties, including a volume resistivity of >1014 ohm-cm and a dielectric constant of 4.8 at 60 Hz. It offers chemical resistance to water, fuels and hydraulic fluids as well as many acids and bases. EP39MAOHT is serviceable from -100°F to +400°F. The combination of these performance properties makes it well suited for application in the aerospace, electronic, electrical, optical and specialty OEM industries.

EP39MAOHT is off-white in color and is available for use in 1/2 pint, pint, quart, gallon and 5 gallon container kits.

Master Bond Thermal Cycling Resistant Adhesives

EP39MAOHT is a toughened, thermally conductive, electrically insulative two component adhesive, sealant, coating and encapsulation compound that is capable of withstanding rigorous thermal cycling. Read more about Master Bond’s thermal cycling resistant adhesives at https://www.masterbond.com/properties/thermal-cycling-resistant-adhesives or contact Tech Support. Phone: +1-201-343-8983 Fax: +1-201-343-2132 Email: [email protected].

About Master Bond
Since its founding in 1976, Master Bond has been committed to developing epoxies, silicones, light curing systems and other specialty adhesives that meet specific customer requirements. Master Bond manufactures over 3,000 grades of specially designed formulations that are widely used across a variety of industries including electronic, medical, aerospace and optical.

Note to Editors:

For a full product description, please visit: http://www.masterbond.com/tds/ep39maoht
Check out product videos on our YouTube channel: http://www.youtube.com/user/MasterBondVideo

You can embed any of our videos on your website.

CONTACT
James Brenner, Marketing Manager
Email: [email protected]
Tel: +1-201-343-8983
Fax: +1-201-343-2132