Master Bond EP3HTS-LO is a single component epoxy for demanding bonding, sealing and coating applications. This system passes ASTM E595 tests for NASA low outgassing, making it well suited for use in the aerospace, electronic, microelectronic and optical industries.
Featuring a silver filler, EP3HTS-LO is electrically conductive with a low volume resistivity of less than 0.001 ohm-cm. It also has a thermal conductivity of 12-15 BTU•in/(ft²•hr•°F) [1.73-2.16 W/(m·K)]. EP3HTS is dimensionally stable and bonds well to metals, glass, composites, ceramics and many plastics. It withstands a variety of chemicals such as water, oils, fuels and cleaning agents. This high temperature resistant system is serviceable over the wide temperature range of -60°F to +400°F.
As a one part compound, EP3HTS-LO offers convenient handling with no mixing and an unlimited working life at room temperature. This smooth thixotropic paste can be readily dispensed from a syringe. It polymerizes quickly at elevated temperatures with cure schedules of 45-50 minutes at 250°F or 20-30 minutes at 300°F.
EP3HTS-LO is available for use in glass jars and syringes. It has a minimum shelf life of 3 months and a maximum of 6 months at ambient temperatures in its original, unopened containers.
NASA low outgassing approved, Master Bond EP3HTS-LO is a single component compound that cures rapidly at elevated temperatures. It offers superior dimensional stability, thermally conductivity and electrical conductivity. Read more about Master Bond’s silver filled, electrically conductive adhesives at www.masterbond.com/properties/silver-filled-electrically-conductive-adhesives or contact Tech Support. Phone: +1-201-343-8983 Fax: +1-201-343-2132 Email: [email protected].
Note to Editors:
For a full product description, please visit: http://www.masterbond.com/tds/ep3hts-lo
Check out new videos on our YouTube channel: http://www.youtube.com/user/MasterBondVideo
You can embed any of our videos on your website.
CONTACT
James Brenner, Marketing Manager
Email: [email protected]
Tel: +1-201-343-8983
Fax: +1-201-343-2132
MASTER BOND INC.
154 Hobart Street
Hackensack, NJ 07601-3922
Web: www.masterbond.com
# # #