Supreme 34CA
Two component epoxy system for bonding, sealing and coating applications
Key Features
- Very high temperature resistance
- Robust resistance to aggressive chemicals
- Very long open time
- Good flow properties
Typical Properties
Viscosity
7,000-20,000 cps
Cure Schedule
gel for 1 hour at 110°C followed by 2-3 hours at 125-150°C
Hardness
>75 Shore D
Service Temperature Range
-80°F to +500°F
Tensile Lap Shear Strength
>2,500 psi
Volume Resistivity
>10¹⁴ ohm-cm