Most Popular Medium Viscosity Adhesives, Sealants, Coatings, Potting/Encapsulation Compounds
High temperature resistant, room temperature curing epoxy system. Exceptional bond strength and dimensional stability. Optically clear. Meets FDA Chapter 1, Section 175.105 requirements. Easy to apply. Serviceable from -60° to +400°F. Protects against exposure to water, oils, fuels, acids, bases and many solvents. Rigid system. Impressive electrical insulation values.
Ultra high temperature resistance up to 300°C. Superb flexibility and elasticity. Non-corrosive. One component, room temperature curing. Flowable.
One part, low viscosity, optically clear system. Fast curing with a high bond strength. Superior dimensional stability and electrical insulative properties. Serviceable from -60°F to +250°F.
Fast, one component heat curable adhesive. Serviceable from -60°F to +400°F. High shear strength properties. Shore D hardness >70. "Unlimited" working life at room temperature. Superb electrical insulator. Withstands 1,000 hours 85°C/85% RH.
High peel and shear strength system. Convenient one to one mix ratio. Serviceable from -100°F to +350°F. Superior resistance to impact, thermal shock, vibration and stress fatigue cracking. Excellent toughness. Cures readily at room temperature. User friendly. Dependable dimensional stability. Readily machinable.
Moderate viscosity, one part UV curing urethane acrylate system that turns from blue to clear upon UV light exposure. Outstanding flexibility and toughness. High bond strength. Serviceable from -80°F to +250°F.
One part, heat curing epoxy with unlimited working life at room temperature. Outstanding chemical resistance, high glass transition temperature, optically clear. For bonding and sealing.