EP21DP11 Red
Two component, low viscosity epoxy for bonding, sealing, coating and potting, colored red
Key Features
- Two to one mix ratio by weight or volume
- Long working time
- Well suited for moderate to large potting
- Good electrical properties
Typical Properties
Viscosity
Part A: 4,000-8,000 cps, Part B: 2,000-5,000 cps
Cure Schedule
75°F: 2-3 days; 200°F: 2-3 hours; Optimal cure: Overnight at 75°F, followed by post cure at 150°F for 2-3 hours.
Hardness
45-55 Shore D
Service Temperature Range
-80°F to +250°F
Dielectric Constant
3.5
Dielectric Strength
440 volts/mil
Volume Resistivity
>10¹⁵ ohm-cm