EP21LP Black
Two component, room temperature curing epoxy compound
Key Features
- Moderate viscosity
- Electrically insulative
- Room temperature curing
- One to one mix ratio — rigid to flexible cure
- Shore D hardness 70-80
- Dimensionally stable
Typical Properties
Viscosity
Part A: 11,000-15,000 cps, Part B: 45,000-65,000 cps
Cure Schedule
75°F: 48-72 hours; 200°F: 2-3 hours
Hardness
70-80 Shore D
Service Temperature Range
-60°F to +250°F
Coefficient of Thermal Expansion
45-50 in/in X 10⁻⁶/°C
Dielectric Constant
2.9
Dielectric Strength
440 volts/mil
Tensile Lap Shear Strength
2,800-3,000 psi
Volume Resistivity
>10¹⁴ ohm-cm
Bild
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
Meets EU Directive 2015/863
Packaging