EP21LP Black

Two component, room temperature curing epoxy compound
Key Features
  • Moderate viscosity
  • Electrically insulative
  • Room temperature curing
  • One to one mix ratio — rigid to flexible cure
  • Shore D hardness 70-80
  • Dimensionally stable
Typical Properties
Viscosity
Part A: 11,000-15,000 cps, Part B: 45,000-65,000 cps
Cure Schedule
75°F: 48-72 hours; 200°F: 2-3 hours
Hardness
70-80 Shore D
Service Temperature Range
-60°F to +250°F
Coefficient of Thermal Expansion
45-50 in/in X 10⁻⁶/°C
Dielectric Constant
2.9
Dielectric Strength
440 volts/mil
Tensile Lap Shear Strength
2,800-3,000 psi
Volume Resistivity
>10¹⁴ ohm-cm
Immagine
EP21LP Black Two Part Epoxy
Certifications

Meets EU Directive 2015/863

Product Description

Master Bond EP21LP Black is a two component, room temperature curing epoxy adhesive, sealant, coating, and encapsulating system featuring outstanding physical properties, superb dimensional stability and low shrinkage upon curing. This moderate viscosity system has a very forgiving 1 to 1 mix ratio by weight or volume. In fact, EP21LP Black has the unusual feature of allowing the properties of the cured system to be altered by tweaking the mix ratio. Adding more Part A (maximum allowed 2:1 mix ratio by weight) will give a more rigid cure, which allows for better machinability. Adding more Part B (maximum 1:2 mix ratio by weight) offers a more forgiving cure, allowing for enhanced impact and shock resistance. It bonds well to a variety of substrates including metals, composites, glass, ceramics and many rubbers and plastics. EP21LP Black features solid thermal cycling resistance. It also withstands many chemicals including water, oils, fuels and many acids and bases. It is serviceable over the wide temperature range of -60°F to +250°F. The color of Part A is black and Part B is amber. Once cured , EP21LP Black is a highly reliable electrical insulator. EP21LP Black is truly a versatile system and can be used in electronic, electrical, aerospace, optical and OEM applications, among others.

Product Advantages

  • Convenient mixing: non-critical 1:1 mix ratio by weight or volume.
  • Variable mix ratio feature allows adjusting the type of cure.
  • First rate physical strength properties.
  • Moderate viscosity; even and smooth flow.
  • Sound dimensional stability; low shrinkage upon curing.
  • Sterling electrical insulation properties.
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.