Typical Properties
Viscosity
Paste
Cure Schedule
250-300°F for 3-4 hours followed by a post cure at 350-400°F for 1-2 hours
Hardness
80-90 Shore D
Service Temperature Range
-100°F to +450°F
T-peel Strength
>10 pli
Tensile Lap Shear Strength
>2,500 psi
Tensile Modulus
350,000-400,000 psi
Bild
Supreme 45HTND Two Part Epoxy
Applications
Certifications

Meets EU Directive 2015/863

Packaging
Product Description

Master Bond Supreme 45HTND is a two component epoxy system featuring an attractive blend of superior physical properties especially shear and peel strengths for high performance structural bonding applications. It has a fine temperature resistance range of -100°F to +450°F. It is 100% reactive and does not contain any solvents or diluents. Supreme 45HTND is primarily formulated to withstand rigorous thermal cycling, especially when bonding dissimilar substrates.

Supreme 45HTND requires elevated temperature curing at a minimum of 250°F. However, Supreme 45HTND has a paste viscosity that will not flow while being cured. The mix ratio is 100 to 30 by weight and is relatively forgiving. Supreme 45HTND bonds well to a wide variety of substrates including metals, ceramics, glass, composites and many plastics and rubber materials. It resists a wide variety of chemicals including water, fuels, oils as well as many acids, bases and solvents. It is a top level electrical insulating system. The color of Part A is black and Part B is brown, although other colors are available. It can be used in challenging electronic, specialty OEM and aerospace applications where the combination of properties mentioned above is needed.

Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.