Supreme 45HTND
Toughened, two component epoxy system for bonding, sealing and coating
Key Features
- Outstanding temperature resistance
- Superior thermal cycling capabilities
- Excellent electrical insulator
- Non-Drip Application Feature
- Very good peel strength
- Exceptionally long working life
Typical Properties
Viscosity
Paste
Cure Schedule
250-300°F for 3-4 hours followed by a post cure at 350-400°F for 1-2 hours
Hardness
80-90 Shore D
Service Temperature Range
-100°F to +450°F
T-peel Strength
>10 pli
Tensile Lap Shear Strength
>2,500 psi
Tensile Modulus
350,000-400,000 psi