Supreme 11HTLP
Toughened, two component epoxy for bonding and sealing
Key Features
- High viscosity system
- Convenient handling
- Wide service temperature range
- Thermal stabilty up to +400°F
- Withstands thermal cycling
- Superb adhesion to many substrates
Typical Properties
Viscosity
Part A: 90,000-120,000 cps, Part B: 60,000-110,000 cps
Cure Schedule
75°F: 48-72 hours; 200°F: 2-3 hours
Hardness
75-85 Shore D
Service Temperature Range
-112°F to +400°F
Coefficient of Thermal Expansion
50-55 X 10⁻⁶ in/in/°C
Tensile Lap Shear Strength
>3,200 psi