EP13 One Part Epoxy System
EP13
One component, heat curing epoxy for structural bonding applications
Dielectric Constant
4.5
Tensile Lap Shear Strength
3,500 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 60-90 minutes at 300-350°F 80-85 Shore D -60°F to +500°F /es/tds/ep13
EP13LTE One Part Epoxy
EP13LTE
One component, heat curing epoxy for structural bonding applications featuring low coefficient of thermal expansion
Coefficient of Thermal Expansion
15-20 X 10⁻⁶ in/in/°C
Glass Transition Temperature (Tg)
155-160°C
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Gap Filling
paste 300-350°F for 1-2 hours; post cure of 2-3 hours at 350-400°F 85-95 Shore D -60°F to +500°F /es/tds/ep13lte
EP13SPND-2 One Part Heat Cure Epoxy
EP13SPND-2
One component, heat curing epoxy for structural bonding applications
Dielectric Constant
4.9
Tensile Lap Shear Strength
3,000 psi
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Gap Filling
paste 300-350°F for 60-90 minutes, post cure at 350-400°F for 2 hours 85-90 Shore D -60°F to +500°F /tds/ep13spnd-2
One Part Epoxy EP15ND-2
EP15ND-2
One part epoxy for testing adhesion or cohesive strength of metallic based flame-sprayed coatings
Tensile Strength
12,000-14,000 psi
Tensile Lap Shear Strength
2,600-2,800 psi
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
paste 300-350°F for 60-90 minutes 80-90 Shore D -60°F to +250°F /es/tds/ep15nd-2
One Part Epoxy System EP17HT
EP17HT
One component epoxy system for bonding, sealing, coating and casting
Glass Transition Temperature (Tg)
200-210°C
Tensile Lap Shear Strength
2,600-2,800 psi at 75°F
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
45,000-75,000 cps Optimum cure schedule is 300°F for 4-6 hours, plus 12-24 hours at 350°F. 80-90 Shore D -80°F to +600°F /es/tds/ep17ht
EP17HT-100 One Part Epoxy Compound
EP17HT-100
One component epoxy system for potting, encapsulation, bonding and sealing applications with a curing temperature of 200-220°F or higher
Dielectric Constant
3.5
Thermal Conductivity
0.58-0.72 W/(m·K)
  • RoHS Compliant
  • Bonding
  • Sealing
  • Encapsulation
  • Potting
  • Casting
40,000-70,000 cps Cures in 60-90 minutes at 200-220°F, or 45-60 minutes at 275-300°F -100°F to +500°F /es/tds/ep17ht-100
EP17HT-3 One Part Snap Curing Epoxy
EP17HT-3
One component, snap-curing epoxy system
Glass Transition Temperature (Tg)
110-120°C
Tensile Lap Shear Strength
1,800-2,000 psi
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Coating
  • Sealing
80,000-130,000 cps 300°F for 8-12 minutes, 350°F for 3-5 minutes 80-90 Shore D -60°F to +400°F /es/tds/ep17ht-3
EP17HTDA-1 One Part Epoxy
EP17HTDA-1
One component, high temperature resistant epoxy system for bonding and sealing
Dielectric Constant
4.3
Glass Transition Temperature (Tg)
130-135°C
  • MIL-STD-883J for Thermal Stability
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Die Attach
200,000-250,000 cps 12-15 minutes at 212°F or 5-6 minutes at 300°F, followed by 2-3 hours at 300°F or 1-2 hours at 350°F 85-95 Shore D -80°F to +525°F /es/tds/ep17htda-1
One Part Die Attach Epoxy EP17HTDA-2
EP17HTDA-2
One component die attach epoxy system with exceptionally high glass transition temperature
Dielectric Constant
4.4
Glass Transition Temperature (Tg)
185-190°C
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Die Attach
>1,000,000 cps 4-5 hours at 300°F or 3-4 hours at 350°F; to optimize properties, use an additional 2-3 hours at 400°F 90-95 Shore D -80°F to +600°F /es/tds/ep17htda-2
One Part Epoxy EP17HTDM-2 Black
EP17HTDM-2 Black
One component, black epoxy for bonding, sealing and specialty dam-and-fill applications
Dielectric Constant
4.6
Glass Transition Temperature (Tg)
180-190°C
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
>800,000 cps 4-6 hours at 300°F, 2-3 hours at 350°F 90-95 Shore D -80°F to +600°F /es/tds/ep17htdm-2-black