EP17HT

One component epoxy system for bonding, sealing, coating and casting
Key Features
  • Serviceable up to 600°F
  • Exemplary chemical resistance
  • Compelling retention of properties at elevated temperatures
Typical Properties
Viscosity
45,000-75,000 cps
Cure Schedule
Optimum cure schedule is 300°F for 4-6 hours, plus 12-24 hours at 350°F.
Hardness
80-90 Shore D
Service Temperature Range
-80°F to +600°F
Glass Transition Temperature (Tg)
200-210°C
Tensile Lap Shear Strength
2,600-2,800 psi at 75°F
Image
One Part Epoxy System EP17HT
Certifications

Meets EU Directive 2015/863

Product Description

Master Bond EP17HT is an extraordinary one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features excellent physical properties, a superb electrical insulation profile and chemical resistance even with heat exposure to 600°F. Its glass transition temperature (Tg) is a resounding 200-210°C. This system is also distinctive in that it has very low exotherm upon curing and can be used in castings and encapsulations well beyond ½ inch in thickness. The minimum curing temperature for EP17HT is 300°F with faster cures attainable at higher temperatures. It should be noted, in order to obtain the optimum properties, a post cure of 2-12 hours at 350°F is recommended.

EP17HT is 100% reactive and contains no solvents or diluents. EP17HT bonds well to similar as well as dissimilar substrates such as metal, ceramics, plastics and composites. It has a impressive resistance to many chemicals such as acids, bases, salts, fuels, oils and many solvents. Shrinkage upon cure is minimal. It is serviceable from -80°F to +600°F. The color of EP17HT prior to cure is milky white, and after cure, it is amber clear. EP17HT retains its exceptional electrical insulation properties, even at higher temperatures. It is widely used in a variety of applications in the aerospace, oil and chemical processing and specialty OEM industries. A paste version, EP17HTND-2, in black is also available.

Product Advantages

  • Single component system; no mixing prior to use
  • Easy application; only positive contact pressure required during heat cure
  • High tensile, lap shear and compressive strength properties
  • 100% reactive. Contains no solvents, diluents or volatiles
  • High temperature resistance, Tg 200-210°C
  • Superior electrical insulation properties, even at higher temperatures
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.