Product Certifications Applications Viscosity Cure Schedule Hardness Temp. Range Link to Content
MasterSil 920-LO One Part Silicone System
MasterSil 920-LO
One part, low outgassing, low stress silicone system for coating, sealing & encapsulating
Dielectric Constant
2.5
Refractive Index
1.43
  • NASA Low Outgassing
  • RoHS Compliant
  • Coating
  • Encapsulation
5,000-10,000 cps Recommended cure time, 75°F: 7 days 25-35 Shore A -175°F to +500°F /es/tds/mastersil-920-lo
MasterSil 921-LO One Part Silicone Compound
MasterSil 921-LO
One part, low outgassing silicone for bonding, sealing, coating & encapsulation
Dielectric Constant
3.1
Elongation
150-250%
  • RoHS Compliant
  • NASA Low Outgassing
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
10,000-15,000 cps Recommended cure time, 75°F: 7 days 25-35 Shore A -175°F to +500°F /es/tds/mastersil-921-lo
MasterSil 922-LO One Part Silicone System
MasterSil 922-LO
One part, low outgassing silicone for bonding, sealing, coating & encapsulation
Elongation
250-350%
Tensile Modulus
200-300 psi
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste Recommended cure time, 75°F: 7 days 40-50 Shore A -175°F to +500°F /es/tds/mastersil-922-lo
MasterSil 970-LO Two Part Silicone Compound
MasterSil 970-LO
Two part, low outgassing addition curing silicone for bonding, potting, sealing & coating
Dielectric Constant
2.8
Elongation
200-250%
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
Part A: 11,000-16,000 cps, Part B: 8,000 - 12,000 cps 4-6 hours at 150°F or 2-3 hours at 180-200°F 25-40 Shore A -120°F to +400°F /es/tds/mastersil-970-lo
MasterSil 971-LO Two Part Epoxy
MasterSil 971-LO
Two part, low outgassing addition curing silicone for bonding, potting, sealing & coating
Tensile Lap Shear Strength
400-800 psi
Tensile Modulus
400-600 psi
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
Part A: 5,000-10,000 cps, Part B: 4,000-8,000 cps 20-40 minutes at 250-300°F or 1-2 hours at 160-200°F -120°F to +400°F /es/tds/mastersil-971-lo
MasterSil 972TC-LO Two Part Silicone System
MasterSil 972TC-LO
Two part, thermally conductive, low outgassing silicone for bonding, potting, coating & sealing
Dielectric Strength
450 volts/mil
Elongation
40-80%
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
30,000-60,000 cps 20-40 minutes at 250-300°F or 1-2 hours at 160-200°F 60-70 Shore A -120°F to +400°F /es/tds/mastersil-972tc-lo
MasterSil 973S-LO Two Part Silicone Compound
MasterSil 973S-LO
Two part, electrically conductive, low outgassing silicone for bonding, sealing and coating
Elongation
50-100%
Volume Resistivity
0.004 ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 25-45 minutes at 250-300°F or 1-2 hours at 160-200°F 80-90 Shore A -120°F to +400°F /es/tds/mastersil-973s-lo
MasterSil 980 Two Part Fluorosilicone Compound
MasterSil 980
Two part, fluorosilicone for high performance bonding, sealing, coating and potting
Dielectric Constant
6.4
Elongation
100-200%
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
moderate flow 30-60 minutes at 260-300°F or 75-90 minutes at 200-250°F 20-30 Shore A -85°F to +465°F /es/tds/mastersil-980
Two Part Silicone MasterSil 981-LO
MasterSil 981-LO

Two component silicone for bonding and sealing meets NASA low outgassing specifications

Coefficient of Thermal Expansion
450-500 x 10⁻⁶ in/in/°C
Refractive Index
1.437
  • RoHS Compliant
  • NASA Low Outgassing
  • Bonding
  • Sealing
12,500-17,500 cps Cures at ambient temperature in 48–72 hours, or more rapidly in 2–4 hours at 135–165°F. For optimal performance, an initial overnight cure at room temperature followed by 2–4 hours at 135–165°F is recommended. 20-30 Shore A -65°F to +400°F /es/tds/mastersil-981-lo
MB297 One Part Ethyl Cyanoacrylate System
MB297
High viscosity ethyl cyanoacrylate with excellent performance profile
Tensile Lap Shear Strength
1,150 psi
Volume Resistivity
>10¹⁵ ohm-cm
  • RoHS Compliant
  • Bonding
2,200-2,400 cps Set up time, 75°F 20-50 seconds (substrate dependent) 70 Shore D -60°F to +250°F /es/tds/mb297

Need Expert Guidance?

Our expert engineers offer one-on-one consultations to help you navigate our extensive material library and find the right solution for your application. We ensure confidentiality and quick turnaround (1-2 business days).