EP112FLAN-1

High performance, two component, heat curing epoxy for potting & encapsulation
Key Features
  • Excellent toughness
  • Outstanding temperature resistance
  • Exquisite thermal conductivity
  • First class dimensional stability
Typical Properties
Viscosity
30,000-65,000 cps
Cure Schedule
2-3 hours at 250°F followed by 5-8 hours at 300°F with a 2 hour post cure at 350°F
Hardness
>85 Shore D
Service Temperature Range
-60°F to +500°F
Coefficient of Thermal Expansion
25-30 X 10⁻⁶ in/in/°C
Dielectric Constant
4.3
Dissipation Factor
0.31
Thermal Conductivity
22-25 BTU•in/(ft²•hr•°F) [3.173-3.6057 W/(m•K)]
Volume Resistivity
>3x10¹⁴ ohm-cm at 25°C, >3x10¹² ohm-cm at 100°C, >3x10¹¹ ohm-cm at 150°C
Imagen
EP112FLAN-1 Two Part Epoxy
Certifications

Meets EU Directive 2015/863

Packaging
Product Description

Master Bond EP112FLAN-1 is a toughened two component, high performance epoxy resin system featuring very good temperature resistance, extraordinarily high thermal conductivity, fine electrical insulation values and sound dimensional stability. The mix ratio is 100:80 by weight. After mixing EP112FLAN-1 has a very long open time of a few days but requires oven curing. A typical cure schedule is 2-3 hours at 250°F followed by 5-8 hours at 300°F with a 2 hour post cure at 350°F, although, a number of variations are possible. Also EP112FLAN-1 is ideal for potting and encapsulation because of its lower viscosity and its advantageous flow properties. The epoxy bonds well to metals, composites, glass, ceramics and many plastics. As mentioned previously, its most prominent features include toughness, solid thermal conductivity, superior electrical insulation properties and ample dimensional stability. The service temperature range is -60°F to +500°F. Another noteworthy property is its toughness which allows it to be utilized in applications where thermal cycling is an important consideration. EP112FLAN-1 has very low exotherm upon curing and is suitable for larger sized castings and potting applications. EP112FLAN-1 is a specialty type product formulated for challenging electrical, electronic applications where high temperature resistance, a degree of toughness and solid electrical insulation along with superlative thermal conductivity is desirable.

Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.