EP132
Two part epoxy for bonding featuring convenient processing and high temperature resistance
Key Features
- Flowable and thixotropic
- Very long open time
- Superior electrical insulation properties
- Excellent physical strength profile
Typical Properties
Viscosity
25,000-45,000 cps
Cure Schedule
2 hours at 125°C followed by 3 hours at 150°C; post cure of 3-4 hours at 350°F
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +550°F
Dielectric Constant
3.29
Glass Transition Temperature (Tg)
205-210°C