EP21TDCN-LO
Durable, two component epoxy for high performance bonding and sealing
Key Features
- Convenient handling
- Good electrical conductivity
- Withstands thermal cycling
- NASA low outgassing approved
Typical Properties
Viscosity
paste
Cure Schedule
Cures readily at 75°F in 3-4 days, or, alternatively, at 150-200°F for 2-3 hours. The optimum cure is overnight at 75°F, followed by 2-3 hours at 150-200°F.
Hardness
80-90 Shore D
Service Temperature Range
-100°F to +275°F
Tensile Lap Shear Strength
1,400-1,600 psi
Volume Resistivity
5-10 ohm-cm
Imagen