EP33ND
Two component, room temperature curing epoxy for bonding and sealing
Key Features
- Thick paste consistency
- Good machinability
- High temperature resistance
- Demonstrated radiation stability at high radiation dosages
- Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
Part A: paste, Part B: paste
Cure Schedule
overnight at 75°F followed by a post cure at 150-200°F for 2-3 hours
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +450°F
Tensile Lap Shear Strength
2,200-2,400 psi
Tensile Modulus
400,000-450,000 psi