EP51M
Two component, ultra fast setting epoxy system for bonding and sealing
Key Features
- Cryogenic serviceablity
- Reliable electrical insulator
- One to one mix ratio, weight or volume
- Rapid curing — fixture time 7-12 minutes at 75°F
- For repair and high speed production
- Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
Part A: 10,000-16,000 cps, Part B: 50,000-75,000 cps
Cure Schedule
3-5 minutes working life, 7-12 minutes fixturing period, 8-16 hours full curing at 75°F
Hardness
55-65 Shore D
Service Temperature Range
4K to +250°F
Dielectric Constant
4.5
Volume Resistivity
10¹⁴ ohm-cm
Imagen
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
1,000 Hours at 85°C/85% RH
Meets EU Directive 2015/863