EP77M-1
Two component, silver conductive epoxy adhesive system
Key Features
- Very low volume resistivity
- Superior chemical resistance
- Higher temperature resistance
- Good physical strength properties
Typical Properties
Viscosity
Part A: >400,000 cps, Part B: 10-35 cps
Cure Schedule
overnight at 75°F followed by 1-2 hours at 150°F
Hardness
70-80 Shore D
Service Temperature Range
-60°F to +300°F
Thermal Conductivity
20-22 BTU•in/(ft²•hr•°F)[2.88-3.17 W/(m•K)]
Volume Resistivity
<10⁻³ ohm-cm