MasterSil 150

Highlight

Two Part, Condensation Cured, Flexible Silicone For Use In Potting And Encapsulation

Typical Properties
Viscosity
13,000 cps
Cure Schedule
Full cure time at 73°F: 24 hours
Hardness
40 Shore A
Dielectric Constant
2.9
Dielectric Strength
18 KV/mm
Dissipation Factor
3 X 10 -3
Volume Resistivity
5 X 10¹⁴ ohm-cm
Imagen
MasterSil 150 Two Part Silicone
Product Description

MasterSil 150 is a two part condensation cured liquid silicone which, after the addition of curing agent 150, cures at room temperature to a tough, resilient silicone rubber potting and encapsulation compound. MasterSil 150 is used for potting and encapsulation of voltage regulators, high voltage transformers, as well as optical and electronic assemblies. Its unique blend of mechanical and electrical properties offer protection to sensitive electronic components and assemblies from dust, moisture, ozone, thermal shock and vibration. Condensation cured silicones are not recommended for applications which are completely sealed prior to full cure. An "escape" path is required to allow for the release of non-hazardous biproducts formed during the mixing process which promotes completion of the curing cycle.

Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.