Supreme 11HT-3A
Toughened, two component epoxy for bonding, sealing and coating
Key Features
- Convenient handling
- Excellent adhesive properties
- Resists thermal cycling
- High temperature serviceability
Typical Properties
Viscosity
Part A: 90,000-120,000 cps, Part B: 2,000-4,000 cps
Cure Schedule
overnight at 75°F followed by 3-4 hours at 150-200°F
Hardness
75-85 Shore D
Service Temperature Range
-100°F to +400°F
Coefficient of Thermal Expansion
45-50 X 10⁻⁶ in/in/°C
Dielectric Constant
5.4
T-peel Strength
10-15 pli
Tensile Lap Shear Strength
2,200-2,400 psi
Tensile Modulus
300,000-350,000 psi
Volume Resistivity
>10¹³ ohm-cm