Supreme 3HTND-2GT
One component, toughened epoxy adhesive, sealant, coating and glob top
Key Features
- Excellent thermal conductivity
- Fast curing
- Withstands thermal cycling and shock
- Serviceable from 100°F to +400°F
Typical Properties
Viscosity
paste
Cure Schedule
Cures in 20-30 minutes at 250°F or in 5-10 minutes at 300°F
Hardness
>75 Shore D
Service Temperature Range
-100°F to +400°F
Coefficient of Thermal Expansion
23-27 X 10⁻⁶ in/in/°C
Dielectric Constant
4.5
Imagen
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
Meets EU Directive 2015/863