High Elongation, Two Component Epoxy System with Excellent Thermal Shock Resistance
Master Bond EP110F8-3 is a two part epoxy system ideal for sealing, encapsulating, potting, and casting applications. “This toughened system provides very good flexibility and possesses a relatively high elongation of 120-150%”, says Rohit Ramnath, Senior Product Engineer. “It offers a low tensile modulus of around 5,000-15,000 psi and a shore A hardness of 40-50 at room temperature.”
EP110F8-3 features excellent thermal cycling and shock resistance, passing 10 cycles from -55°C to +125°C with no signs of cracking. It has a superior electrical insulation profile with a low dielectric constant of 2.67 as well as a low dissipation factor of 0.006, both measured at 75°F for 1 KHz.
EP110F8-3 has a convenient mix ratio of one to two by weight; the color of Part A is clear while the color of Part B is amber. It has a low mixed viscosity of 1,000-2,000 cps and flows readily. Working life for a 100 gram batch is 2-3 days at room temperature and can be cured within a few hours at 250-300°F.
For Editorial Use
Click below to download this release in the format of your choice.
| Élément joint | Taille |
|---|---|
| EP110F8-3.doc (27.5 KB) | 27.5 KB |
| Élément joint | Taille |
|---|---|
| EP110F8-3.txt (6 KB) | 6 KB |
| Élément joint | Taille |
|---|---|
| EP110F8-3.html (3.48 KB) | 3.48 KB |
News Release Images
Click an image to download a high resolution version in JPEG format.