Supreme 3HTND-2CCM
One component, toughened epoxy system for bonding, sealing, coating and encapsulating
Key Features
- Convenient handling and fast curing
- Ideal for glob topping
- Stellar electrical insulation properties
- Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
paste
Cure Schedule
250°F for 20-30 minutes or 300°F for 5-10 minutes
Hardness
80-90 Shore D
Service Temperature Range
-100°F to +400°F
Glass Transition Temperature (Tg)
90°C
Tensile Modulus
250,000-300,000 psi
Image
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
ASTM E595 Compliant
Meets EU Directive 2015/863
1,000 Hours at 85°C/85% RH
Packaging