EP21NS
Two part, moderate viscosity, nanosilica filled epoxy system for bonding, sealing, coating and encapsulation
Key Features
- Convenient mix ratio
- Exceptionally low shrinkage upon curing
- Outstanding dimensional stability
- Extraordinary electrical insulation properties
Typical Properties
Viscosity
50,000-90,000 cps
Cure Schedule
overnight at 75°F, followed by 4-5 hours at 150°F
Hardness
75-85 Shore D
Service Temperature Range
-80°F to +250°F
Dielectric Constant
2.8
Refractive Index
1.55