Supreme 11AOHTMed
Toughened, high strength, two component epoxy for bonding and sealing
Key Features
- Convenient handling
- Thermally conductive & electrically insulative
- Exceptionally high physical strength profile
- Meets ISO 10993-5
Typical Properties
Viscosity
Part A: 200,000-300,000 cps, Part B: paste
Cure Schedule
75°F: 24-36 hours; 200°F: 1-2 hours
Hardness
80-90 Shore D
Service Temperature Range
-112°F to +400°F
Dielectric Constant
4.6
T-peel Strength
15-20 pli