Product Selector

Filters
Applications
Product Type
Product Type
Certifications
Thermal Conductivity
Product Certifications Applications Viscosity Cure Schedule Hardness Temp. Range Link to Content
MasterSil 153AOMed Two Part Medical Grade Silicone
MasterSil 153AOMed
Two part medical grade, thermally conductive, electrically insulating silicone for bonding and sealing
Dielectric Strength
450 volts/mil
Elongation
100-120%
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 200,000-550,000 cps, Part B: 100,000-500,000 cps overnight at 75°F followed by 2-4 hours at 135°F to 185°F 65-75 Shore A -65°F to +400°F /fr/tds/mastersil-153aomed
MasterSil 153Med Two Part Silicone
MasterSil 153Med
Two component, addition cured medical grade silicone for bonding and sealing
Dielectric Strength
450 volts/mil
Elongation
400-500%
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • USP Class VI Medical
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 150,000-300,000 cps, Part B: 50,000-250,000 cps 75°F: 48-72 hours 20-35 Shore A -65°F to +400°F /fr/tds/mastersil-153med
Two Part Silicone MasterSil 153Med Black
MasterSil 153Med Black
Two component, paste consistency, addition cured medical grade silicone for bonding and sealing
Dielectric Strength
450 volts/mil
Elongation
400-500%
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 150,000-300,000 cps, Part B: 50,000-250,000 cps 75°F: 48-72 hours; 200°F: 2-3 hours; Optimum cure: Overnight at 75°F followed by 1 hour at 150-200°F 20-35 Shore A -65°F to +400°F /fr/tds/mastersil-153med-black
MasterSil 155 Two Part Silicone System
MasterSil 155
Two part, graphite filled silicone for high performance bonding, sealing and coating
Elongation
300-400%
Volume Resistivity
20-40 ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 75°F: 6-7 days; 150°F: 2-4 hours; Optimum cure schedule: overnight at 75°F followed by 2-4 hours at 150°F 35-45 Shore A -85°F to +400°F /fr/tds/mastersil-155
MasterSil 157 One Component Silicone
MasterSil 157
Two component, addition curing silicone for potting, encapsulation and sealing
Dielectric Strength
450 volts/mil
Refractive Index
1.43
  • RoHS Compliant
  • Bonding
  • Sealing
  • Encapsulation
  • Potting
  • Coating
  • Gap Filling
Part A: 5,500-6,000 cps, Part B: 100-300 cps 12-24 hours at 75°F, followed by 3-5 hours at 150-200°F 35-45 Shore A -175°F to +500°F /fr/tds/mastersil-157
MasterSil 170 Gel: Two part silicone encapsulant
MasterSil 170 Gel
Two component, addition curing silicone gel for sealing, potting and encapsulation
Dielectric Strength
500 volts/mil
Refractive Index
1.42
  • RoHS Compliant
  • Encapsulation
  • Potting
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
1,000 cps 24-48 hours at ambient temperatures, or in 1-2 hours at 150-170°F 65 mm penetration -67°F to +392°F /fr/tds/mastersil-170-gel
MasterSil 323
Two component, addition cured silicone for bonding, sealing, and small encapsulations
Elongation
150-250%
Refractive Index
1.44
  • RoHS Compliant
  • Bonding
  • Sealing
  • Encapsulation
  • Coating
  • Gap Filling
  • Potting
Part A: 15,000-30,000 cps, Part B: 10,000-25,000 cps 48-72 hours at 75°F or 2-4 hours at 135-165°F 35-45 Shore A -65°F to +400°F /fr/tds/mastersil-323
MasterSil 323Med
Two component, medical grade silicone for bonding and sealing
Acoustical Impedance
1.1 MRayl
Elongation
150-250%
  • RoHS Compliant
  • ISO 10993-5 for Cytotoxicity
  • Bonding
  • Sealing
  • Encapsulation
  • Potting
  • Gap Filling
Part A: 15,000-30,000 cps, Part B: 10,000-25,000 cps 75°F: 48-72 hours; 135-165°F: 2-4 hours; Optimal cure: Overnight at 75°F followed by 2-4 hours at 135-165°F 35-45 Shore A -65°F to +400°F /fr/tds/mastersil-323med
MasterSil 323Med Black Two Part Medical Silicone
MasterSil 323Med Black
Two component, medical grade silicone for bonding and sealing
Dielectric Strength
450 volts/mil
Elongation
150-250%
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
  • Encapsulation
  • Coating
  • Gap Filling
Part A: 15,000-30,000 cps, Part B: 10,000-25,000 cps cures at ambient temperatures in 48-72 hours or in 2-4 hours at 135-165°F; optimum cure is overnight at 75°F followed by 2-4 hours at 135-165°F 35-45 Shore A -65°F to +400°F /fr/tds/mastersil-323med-black
Master Bond MasterSil 323S-LO Silicone System
MasterSil 323S-LO
Two part, silver filled, low outgassing silicone for bonding, sealing and coating
Elongation
50-100%
Volume Resistivity
<0.003 ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: paste, Part B: paste 8-12 hours at 130-150°F, 4-6 hours at 160-180°F or 2-3 hours at 190-210°F 35-55 Shore A -80°F to +400°F /fr/tds/mastersil-323s-lo