MasterSil 323
Two component, addition cured silicone for bonding, sealing, and small encapsulations
Key Features
- Convenient handling
- Optically clear in thin sections
- Low to moderate viscosity
- Excellent strength properties
Typical Properties
Viscosity
Part A: 15,000-30,000 cps, Part B: 10,000-25,000 cps
Cure Schedule
48-72 hours at 75°F or 2-4 hours at 135-165°F
Hardness
35-45 Shore A
Service Temperature Range
-65°F to +400°F
Elongation
150-250%
Refractive Index
1.44