Product Certifications Applications Viscosity Cure Schedule Hardness Temp. Range Link to Content
MasterSil 170 Gel: Two part silicone encapsulant
MasterSil 170 Gel
Two component, addition curing silicone gel for sealing, potting and encapsulation
Dielectric Strength
500 volts/mil
Refractive Index
1.42
  • RoHS Compliant
  • Encapsulation
  • Potting
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
1,000 cps 24-48 hours at ambient temperatures, or in 1-2 hours at 150-170°F 65 mm penetration -67°F to +392°F /fr/tds/mastersil-170-gel
MasterSil 323
Two component, addition cured silicone for bonding, sealing, and small encapsulations
Elongation
150-250%
Refractive Index
1.44
  • RoHS Compliant
  • Bonding
  • Sealing
  • Encapsulation
  • Coating
  • Gap Filling
  • Potting
Part A: 15,000-30,000 cps, Part B: 10,000-25,000 cps 48-72 hours at 75°F or 2-4 hours at 135-165°F 35-45 Shore A -65°F to +400°F /fr/tds/mastersil-323
MasterSil 323Med
Two component, medical grade silicone for bonding and sealing
Acoustical Impedance
1.1 MRayl
Elongation
150-250%
  • RoHS Compliant
  • ISO 10993-5 for Cytotoxicity
  • Bonding
  • Sealing
  • Encapsulation
  • Potting
  • Gap Filling
Part A: 15,000-30,000 cps, Part B: 10,000-25,000 cps 75°F: 48-72 hours; 135-165°F: 2-4 hours; Optimal cure: Overnight at 75°F followed by 2-4 hours at 135-165°F 35-45 Shore A -65°F to +400°F /fr/tds/mastersil-323med
MasterSil 323Med Black Two Part Medical Silicone
MasterSil 323Med Black
Two component, medical grade silicone for bonding and sealing
Dielectric Strength
450 volts/mil
Elongation
150-250%
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
  • Encapsulation
  • Coating
  • Gap Filling
Part A: 15,000-30,000 cps, Part B: 10,000-25,000 cps cures at ambient temperatures in 48-72 hours or in 2-4 hours at 135-165°F; optimum cure is overnight at 75°F followed by 2-4 hours at 135-165°F 35-45 Shore A -65°F to +400°F /fr/tds/mastersil-323med-black
Master Bond MasterSil 323S-LO Silicone System
MasterSil 323S-LO
Two part, silver filled, low outgassing silicone for bonding, sealing and coating
Elongation
50-100%
Volume Resistivity
<0.003 ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: paste, Part B: paste 8-12 hours at 130-150°F, 4-6 hours at 160-180°F or 2-3 hours at 190-210°F 35-55 Shore A -80°F to +400°F /fr/tds/mastersil-323s-lo
MasterSil 415 One Part Silicone Elastomer
MasterSil 415
One component silicone elastomer adhesive for high performance bonding and sealing
Dielectric Strength
500 volts/mil
Elongation
350-450%
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 12-24 hours at 75°F 25-35 Shore A -185°F to +400°F /fr/tds/mastersil-415
MasterSil 705 One Component Silicone
MasterSil 705
One component, silicone elastomer adhesive for high performance bonding and sealing
Dielectric Constant
2.5
Elongation
300-400%
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gasketing
paste Cures at 75°F 25-35 Shore A -75°F to +450°F /fr/tds/mastersil-705
MastersSil 705S One Component Silicone
MasterSil 705S
One component, non-corrosive silicone for bonding and sealing
Elongation
50%
Volume Resistivity
<0.01 ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gasketing
paste Tack-free time, 75°F for 15-20 minutes 70 Shore A -60°F to +400°F /fr/tds/mastersil-705s
MasterSil 705TC One Part Silicone
MasterSil 705TC
One component, non-corrosive silicone for bonding, sealing & coating
Dielectric Constant
4.2
Elongation
70%
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gasketing
paste Tack-free time, 75°F 7 minutes 70-80 Shore A -60°F to +400°F /fr/tds/mastersil-705tc
MasterSil 707FR One Part Silicone System
MasterSil 707FR-NV
One component, room temperature curing, silicone elastomer
Dielectric Constant
3.2
Dielectric Strength
600 volts/mil
  • RoHS Compliant
  • UL 94V-0 Flame Resistant
  • UL 94V-1
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste Tack-free time, 75°F 5-10 minutes 35-45 Shore A -49°F to +221°F /fr/tds/mastersil-707fr-nv