Non-Drip Adhesives
Master Bond’s non-drip formulations feature superior gap filling capabilities while maintaining outstanding bond strength to a variety of substrates. These high viscosity epoxy, polyurethane, silicone, polysulfide and UV curing systems can be applied on vertical surfaces without any sagging.
Image
Common Applications using Non-Drip Adhesive Systems
Master Bond’s non-drip adhesive compounds are employed in a wide range of applications including:
- Filling of large gaps in worn metal surfaces
- Gap sealing in oil, gas, pressure and water tanks
- Bonding of magnet assemblies
- Protective coating for vertically oriented surfaces
Our Most Popular Non-Drip Adhesives, Sealants and Coatings
Image
Two part, room temperature curing epoxy with easy handling and very good physical strength properties. Non-drip paste. For bonding, sealing, coating. One to one mix ratio. Chemically resistant. Gap filling. Variable mix ratio allows adjusting hardness of cure. Low shrinkage. Service temperature range from -60°F to 250°F.
Image
Toughened, non-drip epoxy adhesive featuring high peel and shear strength properties. 100% reactive. Serviceable from 4k to +400°F. No viscosity change over time. Heat curable.
Image
Excellent adhesion to metals and engineering plastics such as polycarbonates, acrylics. Flexible. For bonding, potting, sealing compound. High shear/peel strength. Resists mechanical shocks and vibration. Moderately low exotherm during cure. Serviceable from -100°F to +250°F. Paste consistency.
Image
Non-drip paste. Exceptional chemical resistance to acids. High bond strength. 100 to 50 mix ratio by weight. Formulated to cure at ambient temperatures. Used for coating pumps, storage vessels, tanks. Serviceable from -60°F to +400°F.
Image
High performance aluminum filled epoxy with one to one mix ratio. Excellent bond strength to metal surfaces. Resists many chemicals and thermal cycling. Low shrinkage upon cure. Easy to apply. Flowable paste viscosity. Exceptionally high compressive strength. Superior dimensional stability. Easily machinable. Service operating temperature range from -60°F to +250°F.
Image
Cures rapidly at elevated temperatures. Superior resistance to moisture. Two part epoxy has long pot life at ambient temperatures. High bond strength properties. Reliable electrical insulator. Serviceable from -60°F to +450°F. Shore D hardness 75-85. Thixotropic paste.
Image
Room temperature curing epoxy with high thermal stability. Serviceable from -60°F to +450°F. Thermal conductive/electrically insulative. Paste viscosity. Gap filling. Superior durability. Low CTE. High bond strength. Resists repeated thermal cycling.
Rapid curing, one part epoxy. Meets USP Class VI biocompatibility standards. Non-drip, paste viscosity. High shear strength. Superb resistance to autoclaving, chemical sterilants, radition, EtO. Serviceable from -60°F to +400°F.