EP35AOLV
Two component, thermally conductive, electrically isolating epoxy system for bonding, sealing and potting
Key Features
- Good flow properties
- High temperature resistance
- Withstands aggressive chemicals
- High compressive strength
Typical Properties
Viscosity
50,000-90,000 cps
Cure Schedule
2-3 hours at 300°F followed by a post cure of 3-4 hours at 300-350°F
Hardness
85-95 Shore D
Service Temperature Range
-60°F to +500°F
Glass Transition Temperature (Tg)
165-170°C
Tensile Lap Shear Strength
900-1,100 psi