EP93AOFR
Two component thermally conductive flame retardant epoxy system that complies with FAR standard 14 CFR 25.853(a) for flame retardancy
Key Features
- Tested as per Amendment 25-116 and Part 25 Appendix F
- Passes vertical burn test
- One to one mix ratio
- For bonding, sealing, coating and potting
Typical Properties
Viscosity
30,000-150,000 cps
Cure Schedule
overnight at 75°F followed by 3-4 hours at 150-200°F
Hardness
80-85 Shore D
Service Temperature Range
-80°F to +300°F
Thermal Conductivity
3.5-4.2 BTU•in/(ft²•hr•°F) [0.5-0.6 W/(m•K)]
Volume Resistivity
>10¹⁴ ohm-cm
Image
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
FAR 25.853(a) for Flame Retardancy
Meets EU Directive 2015/863
Packaging