MasterSil 151S
Two part, silver filled, low outgassing silicone for bonding, sealing and coating
Key Features
- Excellent electrical conductivity
- Addition cured type system
- Highly flexible & temperature resistant
- NASA low outgassing
Typical Properties
Viscosity
Part A: paste, Part B: 50-150 cps
Cure Schedule
4-6 hours at 150 to 180°F and 2-3 hours at 190 to 210°F
Hardness
80-90 Shore A
Service Temperature Range
-80°F to +400°F
Elongation
100-150%
Volume Resistivity
0.004 ohm-cm