MasterSil 713
Low viscosity, one component silicone elastomer compound
Key Features
- Fast, room temperature cures
- Ideal for smaller encapsulations
- Well suited for conformal coatings
- Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
2,000-4,000 cps
Cure Schedule
Tack-free time, 75°F, >50% humidity 12-16 minutes
Hardness
20-30 Shore A
Service Temperature Range
-75°F to +400°F
Dielectric Constant
2.5
Elongation
200-300%