Supreme 18TC
Specially formulated one component conductive epoxy adhesive featuring very low thermal resistance properties; meets NASA low outgassing specification
Key Features
- Can be applied in very thin bond lines
- High thermal conductivity
- Unmatched heat transfer capabilities
- Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
paste
Cure Schedule
90 minutes at 250°F or 60 minutes at 300°F
Hardness
80-90 Shore D
Service Temperature Range
4K to +400°F
Glass Transition Temperature (Tg)
135-140°C
Tensile Lap Shear Strength
2,200-2,400 psi
Image
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
ASTM E595 Compliant
1,000 Hours at 85°C/85% RH
Meets EU Directive 2015/863
Packaging
Vidéo
Product Spotlight Supreme 18TC
This video demonstrates the ease of use and impressive properties of Master Bond Supreme 18TC, a one component smooth epoxy paste adhesive. Formulated with a blend of special thermally conductive fillers, this system can be applied in bond lines as t …