Supreme 70CN
Two component, toughened epoxy system for bonding, sealing, coating and potting derived from natural substances
Key Features
- Moderate viscosity
- Superior chemical resistance
- Black colored, optically opaque
- NASA low outgassing
Typical Properties
Viscosity
8,000-12,000 cps
Cure Schedule
overnight at 75°F followed by 4-5 hours at 140-170°F
Hardness
75-85 Shore D
Service Temperature Range
-150°F to +400°F
Dielectric Constant
4.5
Volume Resistivity
>10¹⁴ ohm-cm
Image
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)