UV15-42C
One component UV system for high performance bonding, coating and sealing
Key Features
- Convenient handling
- Translucent
- Excellent toughness
- Non-drip paste viscosity
- Remarkable bonding capabilities
- Exceptionally fast curing
Typical Properties
Viscosity
paste
Cure Schedule
10-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm2
Hardness
>60 Shore D
Service Temperature Range
-65°F to +300°F
Dielectric Constant
4.2
Elongation
10-20%