EP29LP

Two part, very low viscosity epoxy for bonding, sealing, potting and filament winding
Key Features
  • Room temperature curing epoxy
  • Low viscosity
  • Long working life
  • Low exotherm
  • Optically clear
  • Used in large encapsulation applications
Typical Properties
Viscosity
600-1,700 cps
Cure Schedule
Optimum cure schedule: 75°F for 12-24 hours, followed by a post cure of 4-5 hours at 200°F.
Hardness
>75 Shore D
Service Temperature Range
-60°F to +250°F
Dielectric Constant
3.9
Dielectric Strength
450 volts/mil
תמונה
EP29LP Two Component Epoxy
Product Description

Master Bond EP29LP is a two part, high performance epoxy system featuring low viscosity, exceptionally low exotherm and a very long pot life. It has a convenient two to one mix ratio by weight and is formulated to cure at room temperature or faster at elevated temperatures. The working life of a 100 gram mass is greater than 10 hours and when mixing 1 pound, the working life exceeds 5 hours. The extraordinarily long open time is due to the system generating very little heat upon mixing. EP29LP has a formidable array of outstanding physical properties along with superb optical clarity and light transmission. It is a top notch electrical insulator and is ideally suited for moderate to larger castings. It offers superior resistance to a wide range of chemicals including water, acids, bases, oils and fuels. This system also features low shrinkage upon cure. Although it cures rigid, it has reasonably good impact resistance. It bonds well to a wide variety of substrates including metals, ceramics, glass, optical fibers, polyimide, graphite and many rubbers and plastics. The service temperature range is -60°F to +250°F. This system is 100% reactive and does not contain any solvents or diluents. Its long open time, low exotherm and electrical insulation profile allows it to be used in large encapsulations and for filament winding applications. It is widely used in a variety of industries including aerospace, electronic, optical, fiberoptic, specialty OEM and others.

Product Advantages

  • Convenient, non-critical two to one mix ratio by weight
  • Very low viscosity, exceptionally long working life
  • Superior physical strength profile
  • Notable electrical insulation characteristics; ideal for larger potting and encapsulation applications
  • Exquisite optical clarity
  • Desirable adhesive for composites, optical fiber, fiber reinforced materials
  • Exceptionally low shrinkage upon curing
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.