EP30-3
Highly versatile, two part epoxy system for bonding, coating, sealing and casting
Key Features
- Superb optical clarity
- Excellent chemical resistance
- Strikingly high glass transition temperature
- Long working life
Typical Properties
Viscosity
2,000-5,000 cps
Cure Schedule
60-120 minutes at 170°F plus 2-3 hours at 300°F
Hardness
>75 Shore D
Service Temperature Range
-80°F to +450°F
Glass Transition Temperature (Tg)
>325°F
Volume Resistivity
>10¹⁵ ohm-cm